| 引用本文: | 杜佳旭,刘忠军,焦燕妮,雷娟,敖庆波.Cu掺杂TiSi多孔管状膜材料的制备及孔结构表征[J].材料科学与工艺,2026,34(5):46-57.DOI:10.11951/j.issn.1005-0299.20250057. |
| DU Jiaxu,LIU Zhongjun,JIAO Yanni,LEI Juan,AO Qingbo.Preparation and pore structure characterization of Cu-doped TiSi porous tubular membrane materials[J].Materials Science and Technology,2026,34(5):46-57.DOI:10.11951/j.issn.1005-0299.20250057. |
|
| 摘要: |
| 本研究采用离心沉积结合限域原位反应烧结技术制备了Cu掺杂TiSi多孔膜管状材料,旨在探究Cu掺杂量及烧结温度对膜层微观结构、物相组成、孔隙性能及膜基结合强度的影响,并评估Cu掺杂提升Ti5Si3梯度膜层完整性的可行性。使用X射线衍射仪(XRD)、能谱仪(EDS)和扫描电镜(SEM)对多孔材料的物相组成、元素含量和微观形貌进行了分析;利用多孔材料完整性测试仪对样品过滤性能和孔隙性能进行了测试;利用力学试验机测试了管状样品的膜/基结合强度;以检测结果为基础,对限域原位反应烧结机理及物相演变路径进行了简要分析。结果表明:所制备的多孔膜表面主要物相为Ti5Si3,并伴随生成TiO化合物、TiCu及CuO。提高Cu掺杂量和烧结温度,使得膜层逐渐完整,厚度逐渐增加,相对透气系数和最大冒泡孔径都呈下降趋势,膜/基结合强度呈增加趋势;当温度为1 050 ℃时,膜/基结合强度达到了44.06 MPa。 |
| 关键词: TiSi体系 原位反应 多孔膜 Cu掺杂 孔结构 |
| DOI:10.11951/j.issn.1005-0299.20250057 |
| 分类号:TF124 |
| 文献标识码:A |
| 基金项目:陕西省重点研发计划(2022QCY-LL-59);西安石油大学校青年创新团队项目(2019QNKYCXTD12);西安市科技局秦创原转化孵化能力提升项目(24ZHFH0006);西安石油大学研究生创新基金(YCX2413120). |
|
| Preparation and pore structure characterization of Cu-doped TiSi porous tubular membrane materials |
|
DU Jiaxu1, LIU Zhongjun1, JIAO Yanni1, LEI Juan1, AO Qingbo2
|
|
(1. School of Materials Science and Engineering, Xi’an Shiyou University, Xi’an 710065, China;2. State Key Laboratory of Porous Metal Materials (Northwest Institute for Nonferrous Metal Research), Xi’an 710016, China)
|
| Abstract: |
| This study successfully synthesized Cu-doped TiSi porous tubular membrane materials through an integrated approach combining centrifugal deposition with confined in-situ reactive sintering. Structural characterization was performed via Xray diffraction (XRD), energy-dispersive spectroscopy (EDS), and scanning electron microscopy (SEM) to investigate phase composition, elemental distribution, and microstructural evolution. The filtration performance and pore characteristics were systematically evaluated using a porous material integrity tester, while membrane/substrate bonding strength was quantified through universal mechanical testing. The research systematically investigates the effects of Cu doping concentration and sintering temperature on four critical parameters: membrane layer morphology, phase constitution, pore characteristics, and interfacial bonding strength. Key findings reveal that the membrane surface primarily consists of Ti5Si3 matrix phase, accompanied by TiO compounds, TiCu and CuO. As increasing the Cu doping amount and sintering temperature, the membrane thickness gradually increased, the relative permeability coefficient and the maximum bubbling pore size both decreased, and the membrane/substrate bonding strength gradually increased. When the membrane was synthesized at 1 050 ℃, the membrane/base bonding strength reached 44.06 MPa. |
| Key words: TiSi system in-situ reaction porous membrane Cu doping pore structure |