| 引用本文: | 候志强,段书苏,王志佳,张友良,张建经.壳聚糖对MICP碳酸钙沉积效果及拌合固化红黏土的力学性能[J].材料科学与工艺,2026,34(3):27-36.DOI:10.11951/j.issn.1005-0299.20240220. |
| HOU Zhiqiang,DUAN Shusu,WANG Zhijia,ZHANG Youliang,ZHANG Jianjing.Effect of chitosan on the deposition of MICP calcium carbonate and mechanical properties of mix-cured red clay[J].Materials Science and Technology,2026,34(3):27-36.DOI:10.11951/j.issn.1005-0299.20240220. |
|
| 摘要: |
| 由于黏性土孔隙小、渗透性低,采用传统灌浆方法的微生物诱导碳酸钙沉积(MICP)技术难以有效应用,可以尝试采用拌合法来加固黏性土。胶结液的浓度会影响微生物脲酶活性,从而影响碳酸钙产量,而土体加固效果跟碳酸钙生成量有关,为了提高土体强度,可以通过增加碳酸钙的沉积量来实现。本文在胶结液中添加不同含量的壳聚糖,研究其对碳酸钙沉积量的影响。通过菌液和胶结液直接拌合加固红黏土,探讨壳聚糖对土体抗压和抗剪强度的影响。结果表明:在胶结液中掺入壳聚糖能增加微生物诱导出的碳酸钙沉积量;通过一次拌合击实加固试样后放入室内养护,其14 d无侧限抗压强度分别为纯水组979 kPa、微生物组1 547 kPa、壳聚糖-微生物组1 710~1 755 kPa;随着壳聚糖掺量的提升,土体的黏聚力和内摩擦角也逐渐提高;基于XRD和SEM分析表明,在微生物矿化中通过在胶结液中添加壳聚糖能增加方解石晶体的形成。 |
| 关键词: 微生物诱导碳酸钙沉积 红黏土 壳聚糖 拌合法 土体加固 |
| DOI:10.11951/j.issn.1005-0299.20240220 |
| 分类号:TU52 |
| 文献标识码:A |
| 基金项目:海南省院士创新平台项目(YSPTZX202320);海南省自然科学基金资助项目(522CXTD510). |
|
| Effect of chitosan on the deposition of MICP calcium carbonate and mechanical properties of mix-cured red clay |
|
HOU Zhiqiang, DUAN Shusu, WANG Zhijia, ZHANG Youliang, ZHANG Jianjing
|
|
( College of Civil and Architectural Engineering, Hainan University, Haikou 570228, China)
|
| Abstract: |
| Due to the small pore size and low permeability of clayey soils, traditional grouting methods are difficult to effectively apply the microbial-induced calcium carbonate deposition (MICP) technique. To address this limitation, we propose a mixing method to reinforce clayey soils. The concentration of the cementing solution significantly influences microbial urease activity, which governs calcium carbonate production. Since soil reinforcing effect is directly related to calcium carbonate content, increasing its deposition is essential for improving soil strength. In this study, various concentrations of chitosan were introduced into the cementing solution to investigate their effect on calcium carbonate deposition. Red clay soil was reinforced by direct mixing with bacterial and cementing solutions, and the effects of chitosan on compressive and shear strength were evaluated. The results indicate that integrating chitosan into the cementing solution enhanced microbial-induced calcium carbonate deposition. The unconfined compressive strength of mixed and compacted specimens after 14 days under room conditions was 979 kPa for the pure water group, 1 547 kPa for the microorganism group, and 1 710 kPa to 1 755 kPa for the chitosan-microorganism group, respectively. Increasing chitosan dosage resulted in a gradual increase in soil cohesion and internal friction angle. The XRD and SEM analyses confirmed that chitosan addition enhanced calcite crystal formation during microbial mineralization. |
| Key words: microbially induced calcium carbonate deposition red clay chitosan mixing method soil reinforcement |