    Abstract:

    In order to further investigate the effects of hygrothermal ageing on the mechanical behavior of fiber reinforced polymer (FRP)-steel adhesively-bonded joints, based on existing studies, a series of loading tests were carried out on the hygrothermal ageing-treated FRP-steel adhesively-bonded joints by using a roulette wheel loading device, respectively, from six loading conditions, to study the effects of hygrothermal ageing on the ultimate failure loads, failure modes, stiffness and strength failure criteria of the FRP-steel adhesively-bonded joints, comparing results with the unaged adhesively-bonded joints. The results show that hygrothermal ageing significantly reduces the ultimate failure loads of the FRP-steel adhesively-bonded joints to 11.0 kN and 41.9 kN under shear and tensile loading, respectively. Under combined loading, the effect of hygrothermal aging on the ultimate failure loads was less pronounced. The strength failure criteria curves of the aged and unaged FRP-steel adhesively-bonded joints are close to each other. For tensile and tensile/shear combined loading conditions, hygrothermal aging altered the failure modes of FRP-steel adhesively-bonded joints, transitioning from partial interfacial failure between the FRP core plate and the structural adhesive layer to a combination of FRP delamination failure covering the entire structural adhesive bonding area and fiber fracture failure. Hygrothermal ageing significantly reduced the stiffness of the FRP-steel adhesively-bonded joints under all six loading conditions. Therefore, the effects of hygrothermal ageing on the mechanical behavior of FRP-steel adhesively-bonded joints should be fully considered when designing and using FRP-steel adhesively-bonded joints to avoid their structural damage.

    Reference
    Related
    Cited by
Get Citation
Related Videos

Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:April 25,2023
  • Revised:
  • Adopted:
  • Online: October 19,2026
  • Published:
Article QR Code