Q690D高强钢的低周疲劳模型
CSTR:
作者:
作者单位:

(宁波大学 土木工程与未来城市学院,浙江 宁波 315211)

作者简介:

王万祯(1974—),男,博士,教授

通讯作者:

中图分类号:

TU391

基金项目:

宁波市公益性科技计划(2023S101);浙江省自然科学基金(LY24E080001)


A low-cycle fatigue model of Q690D high-strength steel
Author:
Affiliation:

(School of Civil Engineering and Future Cities, Ningbo University, Ningbo 315211, Zhejiang, China)

Fund Project:

undefined

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为计算高强钢在高应变幅作用下(如强震)的低周疲劳寿命,将高强钢低周疲劳裂纹萌生与稳定扩展面积的增速描述为循环加载次数的递增幂函数。通过积分低周疲劳裂纹萌生与稳定扩展面积增速方程,推导出统一计算疲劳裂纹萌生与稳定扩展寿命的高强钢的低周疲劳模型。将椭球面断裂模型作为高强钢低周疲劳裂纹失稳扩展判据和裂尖开裂判据,对Q690D高强钢圆杆在不同高应变幅下(±0.5%,±1.5%,±2.0%,±2.5%,±3.0%)的低周疲劳裂纹扩展进行了理论计算和数值模拟,得到Q690D高强钢圆杆在不同高应变幅下的低周疲劳裂纹萌生与稳定扩展面积。建立满足应力边界条件的高强钢低周寿命模型参数和疲劳断裂面上最大疲劳载荷作用下的名义最大正应力及疲劳载荷幅作用下的正应力幅的函数。根据Q690D高强钢圆杆的低周疲劳试验寿命和数值计算的低周疲劳裂纹萌生与稳定扩展面积,标定Q690D高强钢圆杆在不同高应变幅下的低周疲劳寿命计算式。计算结果表明,标定的Q690D高强钢圆杆的低周疲劳寿命计算式的计算误差为-26.1%~-2.7%。

    Abstract:

    In order to calculate the low-cycle fatigue life of high-strength steel under high strain amplitudes (such as strong earthquakes), this paper described the rate of the initiation and stable propagation area of a low-cycle fatigue crack in high-strength steel as an increasing power function of the number of cyclic loading cycles. By integrating the accelerated growth equations of the crack initiation area and the stable propagation area under low-cycle fatigue, a low-cycle fatigue model for high-strength steel was derived to uniformly calculate the fatigue crack initiation and stable propagation life. By using an ellipsoidal fracture model as a criterion for unstable propagation of the low-cycle fatigue crack and crack tip cracking in high-strength steel, the propagation of the low-cycle fatigue crack in a round rod made of Q690D high-strength steel under different high strain amplitudes (±0.5%, ±1.5%, ±2.0%, ±2.5%, and ±3.0%) was calculated theoretically and simulated numerically. As a consequence, the initiation and stable propagation areas of the low-cycle fatigue crack in the round rod made of Q690D high-strength steel under different high strain amplitudes were calculated. The paper established a function that satisfies the stress boundary conditions, linking the low-cycle life model parameters of high-strength steel to the nominal maximum normal stress under the maximum fatigue load and the normal stress amplitude under the fatigue load amplitude on the fatigue fracture surface. Based on the low-cycle fatigue test life of the round rod made of Q690D high-strength steel and the numerically calculated crack initiation and stable propagation area under low-cycle fatigue, the low-cycle fatigue life calculation formula for the round rod made of Q690D high-strength steel under different high strain amplitudes was calibrated. The calculation results show that the calculation error of the calibrated low-cycle fatigue life calculation formula for the round rod made of Q690D high-strength steel ranges from -26.1% to -2.7%.

    参考文献
    相似文献
    引证文献
引用本文

王万祯. Q690D高强钢的低周疲劳模型[J].哈尔滨工业大学学报,2026,58(10):108. DOI:10.11918/202504074

复制
分享
相关视频

文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2025-04-27
  • 最后修改日期:
  • 录用日期:
  • 在线发布日期: 2026-10-27
  • 出版日期:
文章二维码