考虑骨料特征影响的轻骨料混凝土断裂性能与分析模型
CSTR:
作者:
作者单位:

(长安大学 建筑工程学院,西安 710061)

作者简介:

魏慧(1990—),女,博士,副教授

通讯作者:

中图分类号:

TU528.2

基金项目:

国家自然科学基金面上项目(52378122);陕西省秦创原“科学家+工程师”队伍建设项目(2025QCY-KXJ-091);西安市“科学家+工程师”队伍建设项目(2025JH-KGYB-0032)


Fracture properties and analysis model of lightweight aggregate concrete considering effects of aggregate characteristics
Author:
Affiliation:

(School of Civil Engineering, Chang′an University, Xi′an 710061, China)

Fund Project:

undefined

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    轻骨料混凝土的断裂行为受骨料特征影响显著,为提升轻骨料混凝土的断裂性能并验证现有模型的适用性,通过70个三点弯曲缺口梁试验,采用两种方法计算轻骨料混凝土的断裂能,对比双K断裂模型(DKFM)和离散颗粒断裂模型(DPFM)的适用性,并系统分析轻骨料平均粒径(dave)、体积分数(Va)、骨料强度和砂浆水胶比对材料断裂能(GF)和断裂韧度(KIc)的影响规律。结果表明:各组轻骨料混凝土的断裂路径均呈现“骨料贯穿破坏”特征,轻骨料与普通骨料的增韧阻裂机制存在显著差异;当轻骨料dave≤10 mm时,GF随dave增大而提升,但当dave>10 mm且Va>40%时,混凝土内部缺陷增加导致断裂性能明显降低;提高骨料强度可改善断裂性能,但效果有限;基于不同曲线计算的GF差异较大,GF-CMOD约为GF-WFM的0.71倍;通过提出骨料特征相关函数,并修正虚拟裂纹系数βfic和特征裂纹长度系数βch后,KIc-DPFM与KIc-DKFM的预测结果吻合较好。

    Abstract:

    The fracture behavior of lightweight aggregate concrete (LWAC) is significantly influenced by aggregate characteristics. To improve the fracture properties of LWAC and verify the applicability of established models, this paper conducted seventy three-point bending notched beam tests and adopted two methods to calculate the fracture energy (GF) of LWAC. The paper compared the applicability of the double-K fracture model (DKFM) and discrete particle fracture model (DPFM) and systematically analyzed the effect of lightweight aggregate′s average particle size (dave), volume fraction (Va), aggregate strength, and mortar water-binder ratio on the material′s GF and fracture toughness (KIc). Results indicate that the fracture paths of all groups of LWAC exhibit the characteristic of "aggregate penetration failure", and there exist significant differences in the toughening and crack-inhibiting mechanisms between lightweight and conventional aggregates. When dave≤10 mm, GF increases with the increase in dave. However, when dave>10 mm and Va>40%, the increase in internal defects of concrete results in a significant reduction in fracture properties. Enhancing aggregate strength can improve fracture properties, but the effect is limited. Significant discrepancies are observed between GF values calculated via different methods. Crack mouth opening displacement (GF-CMOD) is approximately 0.71 times that of the work of fracture method (GF-WFM). An aggregate characteristic-related function is proposed to modify the virtual crack coefficient βfic and characteristic crack length coefficient βch, and the predicted results of KIc-DPFM and KIc-DKFM are in good agreement.

    参考文献
    相似文献
    引证文献
引用本文

魏慧,赵兴鑫,吴涛,曾湖斌.考虑骨料特征影响的轻骨料混凝土断裂性能与分析模型[J].哈尔滨工业大学学报,2026,58(10):13. DOI:10.11918/202502032

复制