极地低温下纤维缠绕型玻璃纤维复合材料管混凝土界面黏结性能
CSTR:
作者:
作者单位:

(1.天津大学建筑工程学院,天津300354;2.滨海土木工程结构与安全教育部重点实验室(天津大学),天津300354; 3.北京市既有建筑改造工程技术研究中心(天津分中心),天津300354;4.中国建筑设计研究院有限公司,北京100044)

作者简介:

谢剑(1974—),男,教授,博士生导师

通讯作者:

中图分类号:

TU398.9

基金项目:

国家自然科学基金(9,1)


Bonding behavior of fiber-wound glass fiber reinforced polymer (GFRP) tube and concrete at arctic low temperatures
Author:
Affiliation:

(1.School of Civil Engineering, Tianjin University, Tianjin 300354, China; 2.Key Laboratory of Coast Civil Structure Safety(Tianjin University), Ministry of Education, Tianjin 300354, China; 3.Beijing Engineering Research Center of Existing Building Renovation (Tianjin Branch), Tianjin 300354, China; 4.China Architecture Design and Research Group, Beijing 100044, China)

Fund Project:

undefined

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为揭示纤维缠绕型玻璃纤维复合材料(GFRP)管混凝土在极地等严寒环境下的黏结性能,以试件所处低温水平(T)、径厚比(D/t)、纤维缠绕角度(θ)及界面处理方式为研究参数,设计并完成了18个圆形试件和14个方形试件的静力推出试验。通过试验观察试件的受力破坏形态,获取各试件黏结应力滑移曲线,分析各参数变化对界面黏结性能的影响规律。结果表明:低温作用能显著改善界面黏结性能,且低温作用对圆管黏结性能的提升作用大于方管;随温度降低,界面黏结强度基本呈线性增加;当温度由20 ℃降低至-30 ℃时,界面抗滑移能力有显著提升,但在负温条件下界面黏结刚度变化不大;在低温下,圆形试件黏结强度与径厚比(D/t)呈负相关,方形试件黏结强度受径厚比(D/t)影响不大,但二者界面黏结刚度随D/t的减小均表现为增大后基本稳定的变化趋势;增大纤维缠绕角度有助于提升界面黏结性能;黏砂试件黏结性能显著高于未黏砂试件,并且二者黏结滑移曲线在摩擦滑移段呈现不同的特征。基于试验结果,提出了极地低温下纤维缠绕型GFRP管混凝土界面黏结强度预测模型,可用于极地结构工程的分析与设计。

    Abstract:

    To investigate the bonding performance of fiber-wound glass fiber reinforced polymer (GFRP) tubes and concrete in polar and severe cold environments, a series of static push-out tests were conducted on 18 circular specimens and 14 square specimens. The study parameters included the low-temperature level (T), diameter-to-thickness ratio (D/t), fiber winding angle (θ), and interface treatment methods. The failure modes were observed during the tests, and the bonding stress-slip curves for each specimen were obtained. The influence of varying parameters on the interfacial bonding performance was analyzed. The results indicate that exposure to low temperatures significantly enhances the interface bonding performance, with the improvement in bonding performance being more pronounced for circular tubes compared to square tubes. As the temperature decreases, the bonding strength at the interface generally increases linearly. Specifically, when the temperature drops from 20 ℃ to -30 ℃, there is a notable enhancement in the anti-slip capacity at the interface; however, the bonding stiffness remains relatively unchanged under negative temperature conditions. In low-temperature conditions, the bonding strength of circular specimens shows a negative correlation with the diameter-to-thickness ratio (D/t), while the bonding strength of square specimens is less affected by D/t. Nevertheless, the bonding stiffness at the interface demonstrates an increasing trend that stabilizes as D/t decreases. Additionally, increasing the fiber winding angle contributes to improved interface bonding performance. Specimens with sand-coating exhibit substantially higher bond performance than uncoated specimens, with distinct characteristics observed in the frictional slip segments of their bonding slip curves. Based on the experimental results, a predictive model for the bonding strength of fiber-wound GFRP tube-concrete interfaces under polar low temperature is proposed, which can be utilized for the analysis and design of polar structural engineering.

    参考文献
    相似文献
    引证文献
引用本文

谢剑,张楷,王梦琴,陈斌剑.极地低温下纤维缠绕型玻璃纤维复合材料管混凝土界面黏结性能[J].哈尔滨工业大学学报,2026,58(10):1. DOI:10.11918/202502011